PICKLING FLUID

Liquid product that removes weld slag, annealing scale, grinding dust and iron parts etc., which prevent a proper passivation of the stainless steel.

PICKLING FLUID is a fluid for pickling austenitic stainless steel. It removes weld slag, annealing scale, grinding dust, iron parts etc., which prevent a proper passivation of the stainless steel. PICKLING FLUID may be used only on austenitic stainless steel, as it corrodes other materials.

From the Stainless Steel Treatment category, see also: PICKLING PASTE and PASSIVATING PASTE.

Specifications

Application

Application

PICKLING FLUID is used mainly for pickling installations and tanks. It may be used by circulation, by spray or in immersion baths.

Directions for Use

Pretreatment: Before commencing, clean and degrease the surfaces to be pickled, as this gives the basis for uniform pickling. Use ARR-SAFETY LIQUID for degreasing small metal surfaces. To degrease tanks etc., we advise the use of a 2-4% solution of ARR-SAFETY LIQUID in warm water. After pickling, rinse thoroughly with a jet of water.

Circulation method: Fill the system with cold undiluted PICKLING FLUID. Pickling will take 2 to 6 hours, depending on the degree of soiling and on the kind of austenitic steel. Do not pickle longer than necessary. Drain the system and rinse carefully, preferably with demineralized water. After rinsing, if required, passivation should follow immediately.

Spraying method: Used mainly for very large surfaces and tanks. Use equipment that is not susceptible to acids. The duration of the spray method is 2-6 hours, depending on the amount of soil. After rinsing with plenty of clean water, the surfaces need to be passivated with our product PASSIVATING FLUID.

Immersion bath method: Fill a plastic or plastic lined bath with undiluted PICKLING FLUID. Place the articles to be pickled into the bath and leave them to soak for 1 to 6 hours, depending on the degree of soiling and the kind of austenitic steel. Remove the articles from the bath and spray them with a powerful water jet, preferably with demineralized water. Passivation should follow immediately after spraying.

Note

A protective oxide layer will form on the austenitic stainless steel only if oxidizing conditions are present, for example during long-term rinsing in oxygen rich water or during storage in the open air. In these circumstances the steel passivates automatically.

Because this passive layer takes a long time to develop to the correct thickness, we recommend passivating with PASSIVATING FLUID, particularly if the stainless steel is exposed to corrosive conditions soon after the pickling treatment. Good results are obtained if the object is sprayed / brushed with PASSIVATING FLUID immediately after it has been rinsed.